LAB / WORKSHOP LOG

Experiment, measure, repeat.

3D printing tests, filament analyses, small open-source scripts and local model experiments. Failed results are recorded too.

Click an entry for details
PARAMETERS
MaterialPETG
Layer0.2 mm
Infill40%
Walls3 perimeters
RESULT

Gyroid delivered the highest breaking load at equal weight. The Grid pattern failed early due to layer delamination. Repeat tests are ongoing.

Related note
FILAMENT ANALYSIS

Material comparison

Same test bar, 0.2 mm layers, 40% gyroid infill. Values are relative scores from 1 to 10.

PLA
6/10
PLA+
7/10
PETG
8/10
ABS
7/10
TPU
5/10