LAB / WORKSHOP LOG
Experiment, measure, repeat.
3D printing tests, filament analyses, small open-source scripts and local model experiments. Failed results are recorded too.
PARAMETERS
Drying65°C / 4 hrs
Ambient humidity58%
MeasurementWeight + surface
RESULT
Stringing and surface bubbling were noticeable on the undried spool. After drying, surface quality and layer adhesion recovered.
Related notePARAMETERS
Wall4 lines
Layer0.2 mm
Test72h water
RESULT
No leakage was observed in either material with 4 wall lines; UV resistance testing is ongoing.
Hydroponic farming projectFILAMENT ANALYSIS
Material comparison
Same test bar, 0.2 mm layers, 40% gyroid infill. Values are relative scores from 1 to 10.